Follow us :

cure silicone rubber for mold making

cure silicone rubber for mold making
FOB Price

US $12.60200 - 40,000 kilogram

US $5.9040,001 - 999,999 kilogram

group name
Addition cure silicone rubber
Min Order
200 kilogram
brand name
Hong Ye silicone rubber
model
HY-E642# silicon rubber
Nearest port for product export
Shenzhen, Guangzhou, Xiamen, Shanghai
Delivery clauses under the trade mode
FOB, CFR, CIF
Acceptable payment methods
T/T, L/C, Westem Union
Export mode
Export through agents
update time
Fri, 08 Nov 2013 18:11:36 GMT

Paramtents

  • Grade Standard Industrial Grade,Food Grade

  • Appearance Fluid

  • Application Industrial Mold Making Materials

  • colour customized

  • certificates SGS RoHS

  • material silicone

  • usage making mold

  • origin shenzhen

  • payment T/T W/U L/C

  • sample available

  • type liquid

  • hardness customized

  • MOQ 200KG

Packging & Delivery

  • Min Order200 kilogram

Briefing

cure silicone rubber for mold making
features: favorable hardness, light viscosity low shrinkage

Detailed

cure silicone rubber for mold making    

 

 

Applications,

 

HY- E642# addition molding silicone could be mainly used for making concrete stones, precision molds, PU molds, prototyping, for life casting, fabric finishing, seal for electronic components and solar circuit board, trademark decoration. etc.

 

 

Description

 

HY- E642# addition molding silicone is generally named two-components silicone rubber, Part A is a flowable liquid, part B is the curing agent. It features an exceptional fluidity and good operability. The mixing ratio is 1:1,mainly be suitable for making FDA molds application.

 

Technique Data of HY-E642# molding silicone

 

Model

HY-E642#

Appearance

Translucent or white

Mixing Ratio

1:1

Operating time (Mins 25°C)

30-50

Curing time (Mins 25°C)

3-4h

Hardness (A°)

42±2

Density ( g/cm 3 )

1.08

Viscosity (CS) (Part A)

30000 ± 5000

Viscosity (CS) (Part B)

5000 ± 500

Viscosity (CS) (After mixed)

10000 ± 2000

Tensile-strength( kgf /cm2 )

100 ± 20

Tear-strength (kgf /cm2 )

>15

Elongation-break(%)

350 ± 50

Retractility(%)

≤0.1

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

Frequently asked questions of Molding silicon

Why does the silicone mold get burnt out?

This consequence happens only because you have left out the important notes when using unsaturated resin materials to produce your products. The unsaturated resin produces great heat when added the curing agent. So you must demould the product within 3 minutes to avoid this problem.

 

Need the datasheet and the price of Molding silicon for reference, please feel free to confirm some of your information in advance,

1) What's the material of your products, plaster, resin, cement, wax, or any others, please?

2) What is the size of your products, small(within 30cm), medium(30-60cm) or big(60-200cm), please?3) How about your way of making silicone mold, by pouring way or brushing way, please?

 

Getting your information in details, we will recommend the most suitable Molding silicon with the best price at the first time for your reference.

 cure silicone rubber for mold makingcure silicone rubber for mold making